page_banner

How to solve the dents after welding with intermediate frequency spot welding machines?

When operating a medium frequency spot welding machine, you may encounter a problem where the solder joints have pits, which directly leads to substandard solder joint quality. So what is the reason for this?

IF inverter spot welder

The causes of dents are: excessive assembly clearance, small blunt edges, large volume of molten pool, and liquid metal falling due to its own weight.

Reasons for radial cracks on the surface of solder joints:

1. Insufficient electrode pressure, insufficient forging pressure, or untimely addition.

2. The electrode cooling effect is poor.

Solution:

1. Adjust appropriate welding parameters.

2. Strengthen cooling.